Title: Mechanical Properties of Concrete depending on Cooling Conditions After High Temperature Heating

Author(s): Gyu Yong Kim, Gyeong Choel Choe, Yeon Woo Kang, Tae Gyu Lee

Publication: JCI

Volume: 12

Issue: 3

Appears on pages(s): 82 - 90

Keywords:

Date: 1/1/2014

Abstract:


Japan Concrete Institute, International Partner Access.