Title: Fire Behaviour of Circular Concrete Columns with Restrained Thermal Elongation

Author(s): João Paulo C. Rodrigues, Luís M. Laím, Manfred Korzen

Publication: JCI

Volume: 12

Issue: 9

Appears on pages(s): 289 - 298

Keywords:

Date: 1/1/2014

Abstract: