International Concrete Abstracts Portal

  


Title: Numerical Study on Drying Shrinkage of Concrete Affected by Aggregate Size

Author(s): Ippei Maruyama, Ai Sugie

Publication: JCI

Volume: 12

Issue: 8

Appears on pages(s): 279 - 288

Keywords:

Date: 1/1/2014

Abstract:


Japan Concrete Institute, International Partner Access.