Title: The Effect of Carbon Nano- and Microfibers on Strength and Residual Cumulative Strain of Mortars Subjected to Freeze-Thaw Cycles

Author(s): Andrzej Cwirzen, Karin Habermehl-Cwirzen

Publication: JCI

Volume: 11

Issue: 3

Appears on pages(s): 80 - 88

Keywords:

Date: 1/1/2013

Abstract: