Title: Predicting the Creep Strain of PVA-ECC at High Stress Levels based on the Evolution of Plasticity and Damage

Author(s): Benny Suryanto, Koichi Maekawa, Kohei Nagai

Publication: JCI

Volume: 11

Issue: 2

Appears on pages(s): 35 - 48

Keywords:

Date: 1/1/2013

Abstract:


Japan Concrete Institute, International Partner Access.

View Resource »