Title: Correlation between Permeability of Concrete and Threshold Pore Size obtained with Epoxy-Coated Sample

Author(s): Yuya Sakai, Choji Nakamura, Toshiharu Kishi

Publication: JCI

Volume: 11

Issue: 8

Appears on pages(s): 189 - 195

Keywords:

Date: 1/1/2013

Abstract:


Japan Concrete Institute, International Partner Access.