Title: Durability against Steel Corrosion of HPFRCC with Bending Cracks

Author(s): Shinichi Miyazato, Youichi Hiraishi

Publication: JCI

Volume: 11

Issue: 4

Appears on pages(s): 135 - 143

Keywords:

Date: 1/1/2013

Abstract:


Japan Concrete Institute, International Partner Access.