Title: A Fuzzy Classification System for Evaluating the Health Condition of Marine Concrete Structures

Author(s): Masoud Dehghani Champiri, S. Hossein Mousavizadegan, Faramarz Moodi

Publication: JCI

Volume: 10

Issue: 3

Appears on pages(s): 95 - 109

Keywords:

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access.