International Concrete Abstracts Portal

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Electro-Osmosis Applied for Formwork Removal of Concrete

Author(s): Nassima Goudjil, Yannick Vanhove, Chafika Djelal, Hassina Kada

Publication: JCI

Volume: 10

Issue: 9

Appears on pages(s): 301 - 312

Keywords:

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access.

View Resource » USE YOUR REPAIR SUBSCRIPTION