Title: Blast Resistance of Double-Layered Reinforced Concrete Slabs Composed of Precast Thin Plates

Author(s): Makoto Yamaguchi, Kiyoshi Murakami, Koji Takeda, Yoshiyuki Mitsui

Publication: JCI

Volume: 9

Issue: 2

Appears on pages(s): 177 - 191

Keywords:

Date: 1/1/2011

Abstract:


Japan Concrete Institute, International Partner Access.