Title: Effect of Detailing of Web Reinforcement on the Behavior of Bottle-shaped Struts

Author(s): Dipak Kumar Sahoo, Murali Sagar Varma Sagi, Bhupinder Singh, Pradeep Bhargava

Publication: JCI

Volume: 8

Issue: 3

Appears on pages(s): 303 - 314

Keywords:

Date: 1/1/2010