Title: Experimental Investigation on Shear Cracking Behavior in Reinforced Concrete Beams with Shear Reinforcement

Author(s): Mohamed Zakaria, Tamon Ueda, Zhimin Wu, Liang Meng

Publication: JCI

Volume: 7

Issue: 1

Appears on pages(s): 79 - 96

Keywords:

Date: 1/1/2009

Abstract:


Japan Concrete Institute, International Partner Access.