Title: Mechanical Properties and Durability of Normal and Water Reduced High Strength Grade 60 Concrete Containing Rice Husk Ash

Author(s): Hilmi Bin Mahmud, Muhammad Fakhar Abdul Malik, Rahaimi Abdul Kahar, Muhammad Fauzi Mohd. Zain, Sudharshan Naidu Raman

Publication: JCI

Volume: 7

Issue: 1

Appears on pages(s): 21 - 30