Title: Optimal Maintenance Plan for RC Members by Minimizing Life-Cycle Cost Including Deterioration Risk Due to Carbonation

Author(s): Chien Kuo Chiu, Takafumi Noguchi, Manabu Kanematsu

Publication: JCI

Volume: 6

Issue: 3

Appears on pages(s): 469 - 480

Keywords:

Date: 1/1/2008