Title: Modeling of Carbonation based on Thermo-Hygro Physics with Strong Coupling of Mass Transport and Equilibrium in Micro-pore Structure of Concrete

Author(s): Tetsuya Ishida, Chun-He Li

Publication: JCI

Volume: 6

Issue: 2

Appears on pages(s): 303 - 316

Keywords:

Date: 1/1/2008

Abstract:


Japan Concrete Institute, International Partner Access.