Title: Path-Dependent High Cycle Fatigue Modeling of Joint Interfaces in Structural Concrete

Author(s): Koichi Maekawa, Naoyuki Fukuura, Masoud Soltani

Publication: JCI

Volume: 6

Issue: 1

Appears on pages(s): 227 - 242

Keywords:

Date: 1/1/2008

Abstract:


Japan Concrete Institute, International Partner Access.