Title: Effects of Strain Rate on Tensile Behavior of Reactive Powder Concrete

Author(s): Kazunori Fujikake, Takanori Senga, Nobuhito Ueda, Tomonori Ohno, Makoto Katagiri

Publication: JCI

Volume: 4

Issue: 1

Appears on pages(s): 79 - 84

Keywords:

Date: 1/1/2006

Abstract:


Japan Concrete Institute, International Partner Access.