Title: Simplified Design of Composite Slabs Using Slip Block Test

Author(s): G. Mohan Ganesh, Akhil Upadhyay, Surendra K. Kaushik

Publication: JCI

Volume: 3

Issue: 3

Appears on pages(s): 403 - 412

Keywords:

Date: 1/1/2005

Abstract: