Title: Influence of Bleeding on Minute Properties and Steel Corrosion in Concrete

Author(s): Melito A. Baccay, Takahiro Nishida, Nobuaki Otsuki, Junpei Hamamoto, Kyoku Chin

Publication: JCI

Volume: 2

Issue: 2

Appears on pages(s): 187 - 199

Keywords:

Date: 1/1/2004

Abstract: