Title: Effect of Drying Methods on Microstructural Changes in Hardened Cement Paste: an A. C. Impedance Spectroscopy Evaluation

Author(s): James J. Beaudoin, Basile T. Tamtsia

Publication: JCI

Volume: 2

Issue: 1

Appears on pages(s): 113 - 120

Keywords:

Date: 1/1/2004

Abstract:


Japan Concrete Institute, International Partner Access.