Title: Relation between Strain on Surface and Strain over Embedded Steel Bars in ASR Affected Concrete Members

Author(s): Tarek Uddin Mohammed, Hidenori Hamada, Toru Yamaji

Publication: JCI

Volume: 1

Issue: 1

Appears on pages(s): 76 - 88

Keywords:

Date: 1/1/2003

Abstract:


Japan Concrete Institute, International Partner Access.