Title: Observation of Multiple Cracking in Hybrid FRCC at Micro and Meso Levels

Author(s): Koji Otsuka, Hirozo Mihashi, Masakazu Kiyota, Satoshi Mori, Atsushi Kawamata

Publication: JCI

Volume: 1

Issue: 3

Appears on pages(s): 291 - 298

Keywords:

Date: 1/1/2003