Title: Simultaneous Transport of Chloride and Calcium Ions in Hydrated Cement Systems

Author(s): Takafumi Sugiyama, Worapatt Ritthichauy, Yukikazu Tsuji

Publication: JCI

Volume: 1

Issue: 2

Appears on pages(s): 127 - 138

Keywords:

Date: 1/1/2003

Abstract:


Japan Concrete Institute, International Partner Access.