Title: Overview of ACI 301

Author(s): Michelle L. Wilson

Publication: Web Session

Volume: ws_2017_1009_Wilson_OOA3.pdf

Issue:

Appears on pages(s):

Keywords:

Date: 10/24/2016

Abstract:
This session addresses how to use ACI 301, “Specifications for Structural Concrete,” to comply with ACI 318, Chapter 26, “Construction Documents.”