Title: 345.1R-92: Routine Maintenance of Concrete Bridges (Reapproved 1997)

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 13

Keywords: bridges

Date: 2/1/1992

Abstract:

Note: A newer version of this document exists. This document was replaced by 345.1R-06.

Describes various potential sources of distress and the possible areas affected in the roadway, superstructure, substructure, approaches, slopes and channel of a bridge. Guidance for day-to-day maintenance and preventive maintenance guide. Directed to the maintenance supervisor responsible for routine bridge maintenance.




  