In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Email Support
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Barcelona Test as an Alternative Method to Control and Design Fiber-Reinforced Concrete Pipes
Author(s): Renata Monte, Albert de la Fuente, Antonio Domingues de Figueiredo, and Antonio Aguado
Publication: Structural Journal
Volume: 113
Issue: 6
Appears on pages(s): 1175-1184
Keywords: Barcelona test; concrete pipes; cracking; design; fibers; numerical simulation
Date: 11/1/2016
Abstract:The use of fibers as primary reinforcement for concrete pipes (CPs) is known by both industrial and scientific researchers as an attractive alternative to steel. However, the use of fibers in CPs has not yet been well established in this industry because of, among other reasons, the lack of systematic quality control of fiber-reinforced concrete pipes (FRCPs). Therefore, an experimental program involving the production and testing of 600 mm (23.6 in.) internal-diameter FRCPs was performed using low contents of steel (10 and 20 kg/m3 [0.62 and 1.25 lb/ft3]) and polypropylene (2.3 and 4.6 kg/m3 [0.14 and 0.29 lb/ft3]) fibers. These FRCPs were expected to be viable alternatives to those unreinforced and steel bar-reinforced concrete pipes corresponding to low- to moderate-strength classes. A numerical simulation of the tests using the constitutive equation derived from the Barcelona test was carried out, aimed at confirming that both can be an innovative combination to deal with both the characterization of the FRC tensile behavior and the direct design of these pipes. In this regard, those pipes containing 20 kg/m3 (1.25 lb/ft3)of steel fibers reached the C60 strength class in the TEBT (equivalent to ASTM C76 Class I). Consequently, the steel bars could be completely replaced by fibers. This fact led to an effective reduction of 20% of steel as well as to the elimination of those operations related to the reinforcement preparation. Simultaneously, these FRCPs represent a challenge at a numerical level because the model could be insensitive to this low amount of fibers. The comparisons between the experimental and numerical results have confirmed the suitability of both the model and the constitutive equation to simulate the pipe response when subjected to the TEBT.