Title: Use of Chemical Admixtures to Enable Successful Manufacture of Concrete with Low Portland Cement Content

Author(s): Ara A. Jeknavorian

Publication: Web Session

Volume: Jeknavorian-Ara.pdf

Issue:

Appears on pages(s):

Keywords:

Date: 4/14/2015

Abstract:
The objective of this session will be to address the influence of chemical and mineral admixtures on the early-age properties of concrete, mortar, and grout. The session will educate practitioners on methods to measure early shrinkage, and to examine the effect of admixtures on early-age properties.