Title: Acrylics, Methyl Methacrylate (MMA), and High-Molecular-Weight Methacrylate (HMWM)

Author(s): Richard First, Sales Manager, BASF, Beachwood, OH

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords:

Date: 10/28/2014

Abstract:
This presentation highlights methyl methacrylate (MMA) technology and how it is used to fill and seal concrete cracks.