Title: A Probabilistic Model for Predicting Early-Age Creep Deformation of Self-Consolidating Concrete Members

Author(s): Young Hoon Kim

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

Date: 10/28/2014

Abstract:
The hardened properties and performance of self-consolidating concrete (SCC) developed for use in precast prestressed applications will be discussed. Presentations will specifically focus on SCC mechanical properties, durability, time-dependent behavior, structural behavior, and case studies that document the use of SCC in full-scale precast prestressed applications.


Free Access