Title: 546R-14: Guide to Concrete Repair

Author(s): ACI Committee 546

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 70

Keywords: anchorage; coating; concrete repair; joint sealant; placement; polymer; protective systems; repair materials; structural strengthening.

Date: 9/1/2014

Abstract:
This guide presents recommendations for the selection and application of materials and methods for repairing, protecting, and strengthening concrete structures. An overview of materials and methods is presented as a guide for selecting a particular application. References are provided for obtaining in-depth information on the selected materials or methods.