546.3R-14: Guide to Materials Selection for Concrete Repair

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: 546.3R-14: Guide to Materials Selection for Concrete Repair

Author(s): ACI Committee 546

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 72

Keywords: cementitious; cracks; epoxy; materials; methacrylate; polymer; polyurethane; repair; surface sealer; silica fume; test methods; waterproofing.

Date: 6/1/2014

Abstract:
This document provides guidance on the selection of materials for concrete repair. An overview of the important properties of repair materials is presented as a guide for making an informed selection of the appropriate repair materials for specific applications and service conditions.