SP-293: Reinforced Concrete Columns with High Strength Concrete and steel Reinforcement

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: SP-293: Reinforced Concrete Columns with High Strength Concrete and steel Reinforcement

Author(s): Editor: Halil Sezen / Sponsored by ACI Committtee 441

Publication: Special Publication

Volume: 293

Issue:

Appears on pages(s): 164

Keywords:

Date: 10/4/2013

Abstract:
Practicing engineers increasingly favor the use of high-strength concrete and reinforcement in their design. The paper included in this CD present results from recent research studies and examples of practical applications and use of high-strength concrete and steel reinforcement in recent projects. This CD consists of 10 papers that were presented at a technical session sponsored by ACI Committee 441 at the ACI Convention in Toronto. Ontario, Canada in October 2012. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-293