Shear Behavior of Headed Anchors with Large Diameters and Deep Embedments

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Shear Behavior of Headed Anchors with Large Diameters and Deep Embedments

Author(s): Lee, N. H.; Park, K. R.; and Suh, Y. P.

Publication: 318Reference

Volume: D

Issue: 29

Appears on pages(s): pp. 146-156.

Keywords:

Date: 6/1/2011

Abstract:
ACI Structural Journal, V. 107, No. 2, Mar.-Apr. 2010


Free Access