Displacement-Based Design of Reinforced Concrete Columns for Confinement

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Displacement-Based Design of Reinforced Concrete Columns for Confinement

Author(s): Saatcioglu, M., and Razvi, S. R.

Publication: 318Reference

Volume: 10

Issue: 27

Appears on pages(s): pp. 3-11.

Keywords:

Date: 6/1/2011

Abstract:
ACI Structural Journal, V. 99, No. 1, Jan.-Feb. 2002


Free Access

View Resource »