Effects of Testing Variables on the Strength of High-Strength (90 MPa) Concrete Cylinders

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Effects of Testing Variables on the Strength of High-Strength (90 MPa) Concrete Cylinders

Author(s): Carino, N. J.; Guthrie, W. F.; Lagergren, E. S.; and Mullings, G. M.

Publication: 318Reference

Volume: 5

Issue: 6

Appears on pages(s): pp. 589-632.

Keywords:

Date: 6/1/2011

Abstract:
High-Performance Concrete, SP-149, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1994