THE AUTOGENOUS SHRINKAGE

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: THE AUTOGENOUS SHRINKAGE

Author(s): Públio Penna Firme Rodrigues

Publication: ANAPRE

Volume:

Issue:

Appears on pages(s):

Keywords: AUTOGENOUS SHRINKAGE

Date: 11/1/2009

Abstract:
In this article the author writes about the autogenous shrinkage behavior explaining in a simplified way the physical phenomena involved in the process.