Title: 548.11R-12: Guide for the Application of Epoxy and Latex Adhesives for Bonding Freshly Mixed and Hardened Concretes

Author(s): ACI Committee 548

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 4

Keywords: adhesives; bonding; epoxy adhesives; evaluation; latex adhesive; preparation.

Date: 9/1/2012

Abstract: