Chemical, Biological, and Physical Deterioration Mechanisms in Concrete Piling Along Georgia’s Coastline

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Chemical, Biological, and Physical Deterioration Mechanisms in Concrete Piling Along Georgia’s Coastline

Author(s): Kimberly Kurtis

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: durability, deterioration, piling, coast

Date: 10/19/2011

Abstract:
Concrete durability is often examined one mechanism at a time. For example, freezing-and-thawing attack could be examined or alkali-silica reaction could be examined. But natural exposure conditions can simultaneously subject concrete to multiple attack mechanisms, which can result in a more severe attack than if the mechanisms were evaluated separately. This sessions will present information on the combined effects of different durability mechanisms that could be present at the same time in actual concrete installations.