Title: SP-280: Advances in FRC Durability and Field Applications

Author(s): Editors: Corina-Maria Aldea & Mahmut Ekenel / Sponsored by ACI Committee 544

Publication: Special Publication

Volume: 280

Issue:

Appears on pages(s): 158

Keywords:

Date: 12/29/2011

Abstract:
This CD-ROM contains 10 papers that were presented at sessions sponsored by ACI Committee 544 at the Spring 2011 ACI Convention in Tampa, FL. The topics of the papers cover durability aspects of fiber-reinforced concrete, ranging from permeability, shrinkage cracking, long-term behavior in chloride environment and resistance to chloride penetration, as well as applications of fiber-reinforced concrete for coupling beams for highrise core-wall structures, beams for bridges, panels and suspended foundation slabs. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-280