Title: Self-Sensing Carbon-Nanotube/Cement Composite

Author(s): Xun Yu

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: fiber-reinforced concrete, smart materials, cement-based sensors, self sensing carbon nanotubes

Date: 10/17/2011

Abstract:
This session will include papers on advances on sensing abilities of fiber-reinforced concrete (FRC) and FRC as a smart material. Material suppliers, engineers, researchers, and scientists will benefit from this session.