In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Email Support
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Recent Revisions to Acceptance Criteria for Concrete and Masonry Strengthening Using Externally Bonded FRP Systems
Author(s): Mahmut Ekenel
Publication: Web Session (Outdated)
Volume:
Issue:
Appears on pages(s):
Keywords: masonry, bonded FRP systems
Date: 4/3/2011
Abstract:Unreinforced masonry is vulnerable under loads resulting from seismic activity or blast. This session includes presentations on ACI 440.7R-10, the newly published ACI guideline for strengthening URM walls, and a forthcoming publication on blastresistant components retrofitted with FRP. Additionally, there is a state-of-the-art review on mechanically fastened FRP strengthening systems that uses a new engineered FRP that can provide immediate strength without the need for surface preparation.