Experimental Studies of Mechanically Fastened FRP Systems: State-of-the-Art

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Experimental Studies of Mechanically Fastened FRP Systems: State-of-the-Art

Author(s): Lawrence C. Bank

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: masonry strengthening, FRP

Date: 4/3/2011

Abstract:
Unreinforced masonry is vulnerable under loads resulting from seismic activity or blast. This session includes presentations on ACI 440.7R-10, the newly published ACI guideline for strengthening URM walls, and a forthcoming publication on blastresistant components retrofitted with FRP. Additionally, there is a state-of-the-art review on mechanically fastened FRP strengthening systems that uses a new engineered FRP that can provide immediate strength without the need for surface preparation.