Title: Bond Tests on Concrete Elements Strengthened with EBR and NSM FRP Systems

Author(s): Antonio Bilotta

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: FRP, bond to FRP, EBR, NSM

Date: 4/2/2011

Abstract:
The FRP-to-concrete bond is critically important for the effectiveness of bonded FRP repairs. This session presents the latest theoretical, experimental, and modeling efforts to characterize bond. The topics cover both externally bonded and near-surfacemounted FRP systems.