Title: Influence of the Curvature on the Bond Force Transfer of EBR

Author(s): Wolfgang Finckh

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: FRP, bond force transfer, EBR

Date: 4/2/2011

Abstract:
The FRP-to-concrete bond is critically important for the effectiveness of bonded FRP repairs. This session presents the latest theoretical, experimental, and modeling efforts to characterize bond. The topics cover both externally bonded and near-surfacemounted FRP systems.