Title: Modeling of CFRP-Concrete Interface Subjected to Coupled Pull-out and Push-off Actions

Author(s): Tayyebeh Mohammadi

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: FRP bond to concrete systems

Date: 4/2/2011

Abstract:
The FRP‑to‑concrete bond is critically important for the effectiveness of bonded FRP repairs. This session presents the latest theoretical, experimental, and modeling efforts to characterize bond. The topics cover both externally bonded and near‑surfacemounted FRP systems.