Title: Is the 0.85 Factor Justified for All Concrete Application?

Author(s): Casimir Bognacki

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: core testing

Date: 4/3/2011

Abstract:
Introduction to ACI 214.4R‑10, “Guide for Obtaining Cores and Interpreting Compressive Strength Results.” Attendees will learn how to establish coring programs for new and existing structures and how to evaluate the data obtained. Presentations will include an explanation of the methods presented in the guide.