Title: Noticreto Magazine No. 106, Special Edition: Concrete Solution for Mobility (SPANISH)

Author(s):

Publication: FIHP

Volume:

Issue: 106

Appears on pages(s): 80 pgs

Keywords: Transport systems, mobility, viaduct, brick, tunnel, CO2 emissions, concrete pavements

Date: 5/11/2011

Abstract:
This especial edition (Number 106) of Noticreto Magazine is a compiled of mobility solutions around the world, transport systems implemented in Brazil, Canada, USA, Colombia and other countries in Latin America. Also include technical articles about sustainability in fuel consumption and CO2 emissions using concrete pavements and civil works related with transport systems.


Iberoamerican Federation of Ready Mixed Concrete, International Partner Access.