Title: Hybrid System Design & Construction

Author(s): Jeff Griffin

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: tilt-up, design, mid-rise construction, low-rise construction

Date: 3/22/2010

Abstract:
Tilt-up concrete is both a frontier and a staple in the building industry. Although tilt-up is largely considered an industrial building system, today's market exhibits design and construction accomplishments that are achieved through effective collaboration of architects, engineers, and contractors. This session covers the historical significance of tilt-up design and construction, and the capabilities and technologies that enable the present and future to be dominated by this building method for low- to mid-rise construction.