Blast Performance of Single-Span Precast Concrete Sandwich Wall Panels

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Blast Performance of Single-Span Precast Concrete Sandwich Wall Panels

Author(s): Clay J. Naito

Publication: Web Session (Outdated)

Volume:

Issue:

Appears on pages(s):

Keywords: precast concrete sandwich wall panels, blast and impact

Date: 4/3/2011

Abstract:
This session will provide details of the analysis, design, and performance of precast elements exposed to blast and impact loads. Presentations will include the design considerations, design procedures, and existing resources applicable to the design of precast concrete exposed to blast loads. In addition, current research will be presented detailing the blast and impact resistance of a variety of precast elements. The objective of this session is to provide presentations that detail the state-of-the-art precast concrete designed to resist blast and impact loads. This includes the current procedures being used by engineers to design precast elements and research aimed at material and design advancements.