Title: SP-277: Recent Advances in Maintenance and Repair of Concrete Bridges

Author(s): Editor: Yail J. Kim / Sponsored by: ACI Committee 345

Publication: Special Publication

Volume: 277

Issue:

Appears on pages(s): 199

Keywords:

Date: 3/1/2011

Abstract:
This CD-ROM contains twelve papers that were presented at sessions sponsored by ACI Committee 345 at the ACI Spring 2010 Convention in Chicago, IL. The papers contain information relating to the current technology for concrete bridge repair and maintenance. The papers discussed case studies of damage and corresponding repair, state-of-the-art repair technologies, evaluation and inspection techniques, and maintenance of existing concrete bridges. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-277